Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | Anorthite | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | Barytes, Barite | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Feldspar

An indispensable material in the ceramic industry. Most ceramic bodies employ feldspar as a flux to vitrify them at a lower temperature (the feldspar creates a glass that glues the more refractory particles together to form the fired matrix). Most medium and high-temperature glazes employ it as a flux. They melt, but not too fast, and they help form a durable glass.

Feldspars are naturally occurring crystalline rocks that melt and cool to form a glass (nature cooled them slowly (devitrified them) to form crystalline minerals). There are many kinds of feldspars, but in ceramics, soda, potash and lime feldspars are the most common (technically known as plagioclase, orthoclase and anorthite).

Porcelains can contain up to 50% feldspar, stoneware bodies around 15%. Feldspar sources K2O and Na2O to glazes, these can produce very brilliant results. However, the high KNaO content produces high thermal expansion, which in turn produces crazing. Thus, it is important to control the amount of feldspar and employ materials that source other low-expansion oxides like CaO, MgO, Li2O, BaO, SrO, etc.

Related Information

Links

Glossary Feldspar Glazes
Feldspar is a natural mineral that, by itself, is the most similar to a high temperature stoneware glaze. Thus it is common to see alot of it in glaze recipes. Actually, too much.
Minerals K-Feldspar
Most common feldspars contain both sodium and potassium. The term K-Feldspar designates one where th
Minerals Na-Feldspar
Most common feldspars contain both sodium and potassium. The term Na-Feldspar designates one where t
Oxides K2O - Potassium Oxide
Oxides Na2O - Sodium Oxide, Soda

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.