Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | Anorthite | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Barytes, Barite

Formula: BaSO4

Barite (65.7% BaO, 34.3% SO4) is the main mineral from which barium carbonate is sourced. It is mined around the world and generally occurs in beds or as veins. It is found associated with lead ore, calcite and fluorspar (where it can be identified by its much greater weight). The ore is variously colored and can be quite crystalline in nature. Ground barite is quite chemically inert and fairly inexpensive.

Josiah Wedgewood perfected the use of Barytes as a body and glaze constituent in his Jasper ware.

Barite is relatively soft and easy to grind yet has a very high specific gravity. Its main use is as a weighting agent in drilling mud. Muds with 40% barite have a high enough specific gravity to float debris to the top of the hole during drilling operations.

Related Information

Links

URLs http://en.wikipedia.org/wiki/Barytes
Barytes at Wikipedia
URLs http://www.specialtyminerals.com/our-minerals/what-is-barite-barytes/
What is Barite at specialtyminerals.com
URLs http://www.handbookofmineralogy.org/pdfs/Baryte.pdf
Baryte mineralogy information
Materials Barium Sulfate
Materials Barium Carbonate
A pure source of BaO for ceramic glazes. This is 77% BaO and has an LOI of 23% (lost at CO2 on firing).

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy