1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Zinc Oxide Raw

Alternate Names: Zinc 88, Zinc 90

Formula: ZnO

Oxide Analysis Formula Tolerance
ZnO 88.00% 1.00
LOI 12.00%n/a
Oxide Weight 81.40
Formula Weight 92.50

Notes

Raw zinc oxide has not been calcined so it has some LOI on firing.

Related Information

Frits instead of raw zinc, lithium, barium, strontium


zinc, lithium, barium, strontium oxide powders

This picture has its own page with more detail, click here to see it.

Raw material sources of zinc, lithium, barium, strontium have issues (e.g. precipitates in glaze slurries, toxicity, high drying shrinkage and carbon burnoff that affect laydown and fired surface defects like pinholes, blisters, orange peeling, crystallization). Yet the oxides that these materials supply to the glaze melt - ZnO, Li2O, BaO and SrO, can be sourced from frits which melt much better and remove most of the problems. Consider examples made by Fusion:
-Frit F-493 has 11% Li2O
-F-403 has 35% BaO
-F-581 has 39% SrO
-FZ-16 has 15% ZnO
These frits source other oxides but such are common in most glazes and glaze calculation can be used to retain the overall chemistry. Although these are expensive, the benefits are game changers. But there is a problem: Potters can't get these. Therefore they have difficulty creating the dazzling visual effects of many commercial glazes.

Raw and calcined zinc oxides in a crystalline glaze


This picture has its own page with more detail, click here to see it.

Zinc oxide calcined (left) and raw (right) in typical crystalline glaze base (G2902B has 25% zinc) on typical cone 6 white stoneware body. This has been normally cooled to prevent crystal development. The melting pattern is identical. Note how badly these are crazed, this is common since crystalline glazes are normally high in sodium.

Links

Materials Zinc Oxide
A pure source of ZnO for ceramic glazes, it is 100% pure with no LOI.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy