Pemco Frit P-1V04

Alternate Names: 1V-04,1V04

Description: High sodium low boron low alumina body and glaze flux

Oxide Analysis Formula Tolerance
CaO 6.30% 0.29
K2O 2.30% 0.06
Na2O 15.30% 0.64
B2O3 2.60% 0.10
Al2O3 3.70% 0.09
SiO2 69.80% 3.03
Oxide Weight 260.76
Formula Weight 260.76

Notes

Alkaline-borate flux normally used in wall tile glazes at Cone 1. Sometimes used as engobe or body flux.

Related Information

Links

Materials Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts at very low temperatures. Useful to make crackle glazes.
Materials General Frit GF-134
Materials Fusion Frit F-75
High sodium, high thermal expansion low boron frit. An equivalent of Ferro Frit 3110.
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Keramikos Fritte 31.10
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.9x10-6 (50-450C)
Frit Softening Point 1450F
Frit Melting Range (C) 1400-1550F
Co-efficient of Linear Expansion 9.9x10-6 (50-450C)
I.F.P. (celsius) 605C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy