1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

General Frit GF-134

Alternate Names: Frit 134, Frit GF134

Description: High Alkali Leadless Low Boron

Oxide Analysis Formula Tolerance
CaO 6.26% 0.29
K2O 2.17% 0.06
Na2O 15.27% 0.65
B2O3 2.68% 0.10
Al2O3 3.53% 0.09
SiO2 70.08% 3.06
Oxide Weight 262.50
Formula Weight 262.50

Notes

This frit has a very low melting point.
Low boron for artware glazes and brick coatings. Also used in crystalline glazes.

Related Information

Links

Materials Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts at very low temperatures. Useful to make crackle glazes.
Materials Fusion Frit F-75
High sodium, high thermal expansion low boron frit. An equivalent of Ferro Frit 3110.
Materials Pemco Frit P-1V04
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Keramikos Fritte 31.10
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 10.00
Frit Softening Point 1400F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy