1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Hawthorn Bond

Alternate Names: Hawthorne Fireclay, Hawthorn, Hawthorn 35m, Hawthorne Bond

Description: Missouri Fire Clay

Oxide Analysis Formula Tolerance
CaO 0.25% 0.01 0.25
K2O 0.50% 0.02 0.5
MgO 0.20% 0.02 0.2
Na2O 0.15% 0.01 0.15
TiO2 1.95% 0.08 0.25
Al2O3 31.20% 1.00 0.9
SiO2 50.20% 2.73 3.1
Fe2O3 1.50% 0.03 0.2
LOI 13.00%n/a
Oxide Weight 280.99
Formula Weight 322.98

Notes

Also known as Hawthorn Fireclay or just Hawthorn. It is a popular buff-firing plastic Missouri fireclay of fine particle size and has long been used in many commercial clay body recipes. It fires a buff to tan color with approximately 12% total shrinkage at cone 10. Ground to 35-40 mesh.

This is a different material than AP Green fireclay. The latter is a greenish raw color (this is greyish) and has many more coarse particles in the slurry state. The plasticity of this is such that it can be mixed as-is and used effectively on a potters wheel. Plasticity is quite similar to the AP Green fireclay also. The fired maturity of this is such that it needs only a small amount of feldspar to vitrify in the cone 8-10 range.

Val Cushing recommended Hawthorne as a substitute for Pine Lake Fireclay. However, our testing indicates that although the two have similar porosity over a range of temperatures, this has much higher fired shrinkage and lower drying shrinkage. He also recommended mixing this with 15% Lizella red as a substitute for PBX Fireclay, that is not far off the mark with the latter is a little less vitreous and fires a little darker.

Related Information

Hawthorne fireclay is really more of a stoneware clay


This picture has its own page with more detail, click here to see it.

This is test-result data as reported from an account at Insight-live.com from a test done in 2002. The numbers in the first column in the shrinkage absorption section are the specimen numbers, they bars are labelled (on the right) with them. This clay is already quite dense and vitreous by cone 10 oxidation and reduction (having a 3% porosity), and it has a high fired shrinkage (more than 8%). Drying shrinkage is very low, and its drying factor (performance) is good (even though it is quite plastic). The manufacturer's data sheet shows higher firing shrinkage figures; however, their numbers are actually total fired+drying shrinkage.

What does Hawthorne Firelclay look like when fired?


This picture has its own page with more detail, click here to see it.

This is a Hawthorne Fireclay sample from 1997, these test bars are made to measure fired shrinkage and porosity. Top bar: Cone 10R. Proceeding down from there is cone 11, 10, 8, etc (oxidation). Drying shrinkage is 4.5%. Firing shrinkage is about 8% at cone 11 going down to 7% at cone 6, it is thus very stable across a wide range. Porosity is likewise, 3% at cone 11 slowly rising to 5% by cone 6. So this material is already fairly vitreous by cone 6 yet still stable at cone 11.

Links

Materials NAT Dry Milled Fireclay
Materials Fireclay
Materials APG Missouri Fireclay
Materials Pine Lake Fireclay
Materials Plainsman Fireclay
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
URLs https://christyminerals.com/wp-content/uploads/2020/04/Hawthorn-Bond-Christy-Minerals.pdf
Hawthorne Bond data sheet (from Christy Minerals)

Data

Pyrometric Cone Equivalent 31-32

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy