NAT Dry Milled Fireclay

Description: Buff Burning Plastic Fireclay

Oxide Analysis Formula Tolerance
CaO 0.40% 0.02
MgO 0.40% 0.03
Fe2O3 1.40% 0.03
Al2O3 30.80% 1.00
SiO2 52.00% 2.87
TiO2 1.60% 0.07
LOI 12.30%n/a
Oxide Weight 286.79
Formula Weight 327.02

Related Information

Links

Materials Hawthorn Bond
Materials APG Missouri Fireclay
Materials Kaiser Missouri Fireclay
Materials Fireclay
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy