1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Calcium Feldspar

Alternate Names: Lime Spar, Lime Feldspar, Ca-Feldspar

Formula: CaO.Al2O3.4SiO2 or CaAl2Si2O8

Oxide Analysis Formula Tolerance
CaO 10.82% 1.00
Al2O3 19.66% 1.00
SiO2 69.52% 6.00
Oxide Weight 518.48
Formula Weight 518.48

Notes

Feldspars are roughly divided into lithium, potash, soda, and calcium according the to fluxing oxide that predominates (theoretical formulae for each type are not found in nature). Calcium feldspars are not common and never near theoretical. Thus even if the CaO does not predominate over the K2O and Na2O it may still be labeled a Ca-Feldspar if there is an appreciable amount.

Related Information

Links

Hazards Feldspar
Feldspars are abundant and varied in nature. They contain small amounts of quartz (while nepheline syenite does not).
Minerals Anorthite
A plagioclase feldspar (vs. typical alkali feldspars used in ceramics). More precisely, it is a calc
URLs http://www.webmineral.com/data/Anorthite.shtml
Anorthite info at webmineral.com
Materials Feldspar
In ceramics, feldspars are used in glazes and clay bodies. They vitrify stonewares and porcelains. They supply KNaO flux to glazes to help them melt.
Materials Potash Feldspar
A feldspar having a KNaO content that predominates in potassium.
Materials SP-G Feldspar
Materials Sil-o-spar
Typecodes Generic Material
Generic materials are those with no brand name. Normally they are theoretical, the chemistry portrays what a specimen would be if it had no contamination. Generic materials are helpful in educational situations where students need to study material theory (later they graduate to dealing with real world materials). They are also helpful where the chemistry of an actual material is not known. Often the accuracy of calculations is sufficient using generic materials.
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
Oxides CaO - Calcium Oxide, Calcia

Data

Hardness (Moh) 6-7
Frit Softening Point 1550C
Density (Specific Gravity) 2.7-2.8

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy