Bone Ash Calcined

Formula: Ca3(PO4)2

Oxide Analysis Formula Tolerance
CaO 54.24% 0.75
P2O5 45.76% 0.25
Oxide Weight 77.56
Formula Weight 77.56

Related Information

Links

Materials Tricalcium Phosphate
Materials Bone Ash
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Typecodes Opacifier
Opacifiers are powders that turn transparent glazes opaque by various chemical and physical mechanisms (and combinations of mechanisms).

Data

Frit Softening Point 1670C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy