March 2026: We are doing major upgrades to code here, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.

Monthly Tech-Tip from Tony Hansen SignUpFeb 14-15, 2026 - Major Server Upgrade Done

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit F-65

Alternate Names: Fusion Frit F65

Description: High barium boron frit for cone 06-1 glazes

Oxide Analysis Formula Tolerance
BaO 27.50% 0.65
Na2O 6.00% 0.35
B2O3 13.00% 0.68
Al2O3 5.50% 0.20
SiO2 48.00% 2.89
Oxide Weight 362.11
Formula Weight 362.11

Related Information

Links

Materials Ferro Frit 3289
Materials Pemco Frit P-626
Materials Ferro Frit FB-284-M
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 400
Hazards Barium Carbonate in Glazes
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.85
Frit Softening Point 1450F