1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Frit 3289

Alternate Names: F3289

Description: High barium leadless frit for bright colors, satin finishes

Oxide Analysis Formula Tolerance
BaO 27.40% 0.67
Na2O 5.50% 0.33
B2O3 12.40% 0.67
Al2O3 5.40% 0.20
SiO2 49.30% 3.07
Oxide Weight 373.91
Formula Weight 373.91

Notes

This is a high barium frit. Toxicities are implied by this, be careful about use on functional surfaces. As of 2020 this frit can be purchased at lagunaclay.com.

Related Information

Links

Materials Ferro Frit FB-284-M
Materials Hommel Frit 400
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials General Frit GF-129
Materials Pemco Frit P-658
Materials Pemco Frit Pb-545
Materials Fusion Frit F-65
Materials Pemco Frit P-626
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Hazards Barium Carbonate in Glazes

Data

Co-efficient of Linear Expansion 8.20
Frit Melting Range (C) 1500F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy