Ferro Frit FB-284-M

Alternate Names: Frit 284M, FB284M, FB284-M, FB-284M

Description: Barium Frit

Oxide Analysis Formula Tolerance
ZrO2 1.80% 0.05
SiO2 47.50% 2.96
B2O3 12.40% 0.67
Al2O3 5.40% 0.20
Na2O 5.50% 0.33
BaO 27.40% 0.67
Oxide Weight 373.91
Formula Weight 373.91

Notes

In 2014, this is the only barium frit that Ferro is selling.
Useful in barium matte floor tile glazes, partially fritted satin matte glazes.
Barium source for bright colors cone 05-03.
This is a replacement for Frit 3289, it has 1.8% ZrO2 in place of that much silica.

Related Information

Links

Materials Ferro Frit 3289
Materials Ferro Frit CC-257
Materials Hommel Frit 4GF56E
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-626
Materials Fusion Frit F-65
Materials Degussa Frit 90420
Typecodes Available from Laguna Clays
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Hazards Barium Carbonate in Glazes

Data

Frit Softening Point 1500F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy