Alternate Names: Fusion Frit F2
Description: High Calcium Boron Leadless
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 10.50% | 0.68 | |
| Na2O | 3.00% | 0.18 | |
| B2O3 | 20.30% | 1.06 | |
| Al2O3 | 13.50% | 0.48 | |
| SiO2 | 49.00% | 2.97 | |
| K2O | 3.70% | 0.14 | |
| Oxide Weight | 363.86 | ||
| Formula Weight | 363.86 | ||

This picture has its own page with more detail, click here to see it.
Ferro Frit 3195 and Fusion Frit F-2 are examples of frit made by two different manufacturers yet have similar chemistries and are often sold as substitutes for each other. This melt fluidity test compares them at cone 06. Melt flows like this can tell one many things. For example, Frits are not supposed to have an LOI, it is not clear why both, but especially F-2, have so many entrained bubbles.
| Materials |
Ferro Frit 3195
A commonly used boron frit, it is a balanced glaze all along at cone 06-02 (with the addition of 10-15% kaolin). Not fully glossy. |
| Materials |
General Frit GF-115
|
| Materials |
Pemco Frit P-67
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 399
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.19 |
|---|---|
| Frit Softening Point | 1600F |