Pemco Frit P-67

Alternate Names: Frit 67, Frit P67, Pemco 67

Description: Sodium-potassium-alumina-borosilicate flux

Oxide Analysis Formula Tolerance
CaO 12.50% 0.69
K2O 3.60% 0.12
Na2O 3.80% 0.19
B2O3 26.00% 1.16
Al2O3 12.10% 0.37
SiO2 42.00% 2.17
Oxide Weight 310.25
Formula Weight 310.25

Related Information

Links

Materials Ferro Frit 3195
A commonly available calcium borosilicate frit. It is glaze-like, needing only a kaolin addition to create a low-temperature semi-glossy glaze.
Materials Fusion Frit F-2
Materials General Frit GF-115
Materials Pemco Frit P-54
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 2GF56A
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.0 x 10-6 (50-450C)
Co-efficient of Linear Expansion 7.0 x 10-6 (50-450C)
Frit Melting Range (C) 1530-1760F
I.F.P. (celsius) 675C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy