Fusion Frit F-2

Alternate Names: Fusion Frit F2

Description: High Calcium Boron Leadless

Oxide Analysis Formula Tolerance
CaO 10.50% 0.68
Na2O 3.00% 0.18
B2O3 20.30% 1.06
Al2O3 13.50% 0.48
SiO2 49.00% 2.97
K2O 3.70% 0.14
Oxide Weight 363.86
Formula Weight 363.86

Related Information

Ferro Frit 3195 vs. Fusion Frit F-2 at cone 06


Frit 3195 vs Frit F-2

This picture has its own page with more detail, click here to see it.

Ferro Frit 3195 and Fusion Frit F-2 are examples of frit made by two different manufacturers yet have similar chemistries and are often sold as substitutes for each other. This melt fluidity test compares them at cone 06. Melt flows like this can tell one many things. For example, Frits are not supposed to have an LOI, it is not clear why both, but especially F-2, have so many entrained bubbles.

Links

Materials Ferro Frit 3195
A commonly available calcium borosilicate frit. It is glaze-like, needing only a kaolin addition to create a low-temperature semi-glossy glaze.
Materials Hommel Frit 399
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-67
Materials General Frit GF-115
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.19
Frit Softening Point 1600F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy