Hommel Frit 259

Description: Leadless, use for cone 06-02

Oxide Analysis Formula Tolerance
CaO 0.27% 0.02
K2O 6.04% 0.21
Na2O 14.14% 0.74
ZnO 0.94% 0.04
B2O3 16.50% 0.77
Al2O3 11.75% 0.37
SiO2 48.91% 2.64
F 1.45% 0.25
Oxide Weight 324.10
Formula Weight 324.10

Related Information

Links

Materials Ferro Frit 3819
Materials Pemco Frit P-25
Materials General Frit GF-114
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3269
Materials Fusion Frit FZ-25
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 10.30
Co-efficient of Linear Expansion 10.2 x 10-6
Frit Softening Point 1500F
Frit Melting Range (C) 1500F
By Tony Hansen