Keramikos Fritte 31.10

Alternate Names: CH179E

Description: Natriumsilicaat Fritte, sodium frit

Oxide Analysis Formula Tolerance
CaO 6.28% 0.29
K2O 2.18% 0.06
B2O3 2.42% 0.09
SiO2 70.27% 3.06
Na2O 15.31% 0.65
Al2O3 3.54% 0.09
Oxide Weight 261.77
Formula Weight 261.77

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts at very low temperatures. Useful to make crackle glazes.
Materials General Frit GF-134
Materials Hommel Frit 529
Materials Ferro Frit 4110
Materials Pemco Frit P-1V04

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy