1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ravenscrag Slip 1900F Calcined

Alternate Names: Ravenscrag Slip Calcined

Description: Silty fusible low iron clay

Oxide Analysis Formula Tolerance
BaO 0.30% 0.01
MgO 1.90% 0.16
CaO 11.10% 0.68
K2O 3.30% 0.12
Na2O 0.50% 0.03
TiO2 0.40% 0.02
SiO2 67.80% 3.89
Fe2O3 0.90% 0.02
Al2O3 13.80% 0.47
Oxide Weight 344.76
Formula Weight 344.76

Notes

The chemistry of this material is slightly different than for raw Ravenscrag Slip (it does not lose any weight on firing, so it supplies more of each of the oxides to the fired glaze, 9% more). This chemistry provided here assumes complete calcination (to at least cone 04). However there is an issue. The page at ravenscrag.com recommends roasting to only 1000F, at that temperature it looses only 3% weight on firing.

Another issue is particulates. When calcined at 1900F, particles sinter together into larger ones, requiring glaze ball milling. But at 1000F this does not occur.

Related Information

Ravenscrag Slip + 10% talc = fantastic cone 10R silky matte glaze


Two mugs with silky matte glaze

This picture has its own page with more detail, click here to see it.

The clays are Plainsman H450 and H550. Firing is cone 10 reduction. A 50:50 mix of roasted and raw Ravenscrag slip was used. L3954N black engobe was applied at leather hard stage (on the insides and partway down the outsides). We call this recipe GR10-C Ravenscrag Talc Matte, it is on the insides of both and on the outside of the one on the left. The outside of the other is G2571A Bamboo, it is also an excellent matte base. The silky matte surfaces produced by these two are both functional (they are very durable and do not stain or cutlery mark). And they are very pleasant to the touch.

Links

URLs http://ravenscrag.com
Ravenscrag web site
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
Materials Ravenscrag Slip
A light-colored silty clay that melts to a clear glaze at cone 10R, with a frit addition it creates a good base for a wide range of cone 6 glazes.
Materials Ravenscrag Slip 1000F Roast

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy