Body Color | Body Maturity | Body Plasticity | Body Thermal Expansion | Crystal Glaze Variations | Deflocculant | Glaze Color | Glaze Crystallization | Glaze Matteness | Glaze Opacifier | Glaze Surface Texture | Glaze Suspender | Glaze Variegation

Body Thermal Expansion Property

Materials in this class are added to bodies to reduce their thermal expansion by simply diluting a high expansion matrix by introducing particles having low expansion. It is thus implied that these materials are added as grog and are not fired high enough to change their mineralogy and therefore thermal expansion properties.

Mechanisms

Materials Alkatrol
Materials Pyrotrol 2253
Materials Pyrotrol 3503
Materials Pyrotrol
Materials Mullite
Materials Kyanite
Materials Talc
Materials Pyrophyllite
Materials Calcined Alumina
Materials Zircon
Materials Calcined Kaolin
Materials Andalusite

Links

Glossary Thermal Expansion in Ceramic Bodies and Glazes
The co-efficient of thermal expansion of ceramic bodies and glazes determines how well they fit each other and their ability to survive sudden heating and cooling without cracking.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy