Pyrotrol 3503

Description: Andalusite/Pyrophyllite Ore

Oxide Analysis Formula Tolerance
K2O 0.40% 0.02
Na2O 0.40% 0.03
TiO2 0.40% 0.02
Al2O3 20.50% 1.00
SiO2 75.50% 6.25
Fe2O3 0.40% 0.01
LOI 2.80%n/a
Oxide Weight 485.62
Formula Weight 499.61

Notes

The Pyrotrol group of mineral products offers a controlled blend of milled Andalusite/Pyrophyllite ores designed to control strinkage in whiteware ceramic applications. Alumina contents are controlled to meet certain specifications. Pyrotrol produces an excellent kiln car wash and is an inexpensive coating material for facebrick production.

Related Information

Links

Materials Pyrotrol

Data

Bulk Density lbs/cu. ft. (Packed) 40
Pyrometric Cone Equivalent 26
Sieve Analysis Dry +325 mesh: 1%
Density (Specific Gravity) 2.80

Mechanisms

Body Thermal ExpansionPyrotrol products impart higher strength in electrical porcelains and reduce dunting problems associated with traditional porcelain bodies if substituted for silica content.