Ag2O | AlF3 | As2O3 | As4O6 | Au2O3 | BaF2 | BeO | Bi2O3 | CaF2 | CdO | CeO2 | Cl | CO | CrO3 | Cs2O | CuCO3 | Dy2O3 | Er2O3 | Eu2O3 | F | Fr2O | Free SiO2 | Ga2O3 | GdO3 | GeO2 | HfO2 | HgO | Ho2O3 | In2O3 | IrO2 | KF | KNaO | La2O3 | Lu2O3 | Mn2O3 | MoO3 | N2O5 | NaF | Nb2O5 | Nd2O3 | Ni2O3 | OsO2 | Pa2O5 | PbF2 | PdO | PmO3 | PO4 | Pr2O3 | PrO2 | PtO2 | RaO | Rb2O | Re2O7 | RhO3 | RuO2 | Sb2O3 | Sb2O5 | Sc2O3 | Se | SeO2 | Sm2O3 | Ta2O5 | Tb2O3 | Tc2O7 | ThO2 | Tl2O | Tm2O3 | Trace | U3O8 | UO2 | WO3 | Y2O3 | Yb2O3

MnO2 (Manganese Dioxide)

Data

Co-efficient of Linear Expansion 0.050

Notes

-Manganese dioxide exists only below 1080C, above which the dioxide form disassociates to release its oxygen (see MnO for more information).

-Manganese is a colorant using in bodies and glazes, producing blacks, browns, and purples.

-Manganese is a constituent in many igneous rocks, and thus occurs in many clays weathered from these parent rocks. In most cases it is a very minor oxide, but does occur in much greater amounts in some slip and highly stained materials. It is thus a color contributor in many traditional and historic slip glazes.

-Smaller amounts are easily dissolved in most glaze melts, however, around the 5% threshold, the manganese will precipitate and crystallize. In large amounts in a glaze (i.e. 20%), metallic surfaces are likely.

-In glazes below 1080C, it can give coffee color browns when used with tin.

Ceramic Oxide Periodic Table

Periodic table of ceramic oxides

Pretty well all common traditional ceramic base glazes are made from less than a dozen elements (plus oxygen). Go to the full picture of this table and click or tap each of the oxides to learn more (on its page at digitalfire.com). When materials melt, they decompose, sourcing these elements in oxide form. The kiln builds the glaze from them, it does not care what material sources what oxide (assuming, of course, that all materials do melt or dissolve completely into the melt to release those oxides). Each of these oxides contributes specific properties to the glass. So, you can look at a formula and make a good prediction of the properties of the fired glaze. And know what specific oxide to increase or decrease to move a property in a given direction (e.g. melting behavior, hardness, durability, thermal expansion, color, gloss, crystallization). And know about how they interact (affecting each other). This is powerful. A lot of ceramic materials are available, hundreds - that is complicated when individual materials source multiple oxides. Viewing a glaze as a simple unity formula of ceramic oxides is just simpler.

Links

Materials Manganese Dioxide
A source of MnO used in ceramic glazes and the production of ceramic stains. Commonly made by grinding pyrolusite rock.
Materials Stain
Articles An Overview of Ceramic Stains
Understanding the advantages of disadvantages of stains vs. oxide colors is the key to choosing the best approach
Glossary Limit Formula
A way of establishing guideline for each oxide in the chemistry for different ceramic glaze types. Understanding the roles of each oxide and the limits of this approach are a key to effectively using these guidelines.

Mechanisms

Glaze ColorManganese and cobalt mixture produce black. Iron can also be used. For example, a mix of 8 iron, 4 manganese dioxide and 0.5 cobalt make a raw black stain.
Glaze ColorPurple colors can be produced in glazes of high alkali (KNaO) and low alumina, especially in combinations with cobalt (look for a frit with this profile for best results).

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy