Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | Anorthite | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | Barytes, Barite | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Pyrophyllite

Formula: AlSi2O5OH

Pyrophyllite is an aluminum silicate mineral with a similar chemical structure to talc (a magnesium silicate). It is non-plastic yet clay-like and often used in ceramic bodies to decrease thermal expansion and moisture expansion during service. It is a very soft white mineral (also resembling talc in physical appearance and feel).

Three types are found in nature:
-Micaceous foliated pyrophyllite (flaky with some fluxes).
-Crystalline (higher expansion and longer needle-like grains).
-Homogeneous variety known as massive pyrophyllite. It is used in refractories because it lacks fluxes and has a rounded grain with high lubricity that lends itself to pressing bodies. This type typically has a permanent expansion of about 2% to 2000F.

Phyrophyllite can be variable in nature, so factory blending and select mining are normal. Many other minerals can be found associated with it (e.g. kyanite, andalusite, topaz, quartz, sericite, chlorotoid, pyrite, chlorite, feldspar, hematite, magnetite).

Some grades of Phyrophyllite can be variable in nature, so factory blending and select mining are normal. Many other minerals can be found associated with it (e.g. kyanite, andalusite, topaz, quartz, sericite, chlorotoid, pyrite, chlorite, feldspar, hematite, magnetite).

Related Information

Links

Materials Andafrac
Materials Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc.
Minerals Andalusite
A low expansion alumina silicate mineral.
URLs http://en.wikipedia.org/wiki/Pyrophyllite
Pyrophyllite at Wikipedia

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy