| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| B2O3 | 0.10% | - | |
| CaO | 8.54% | 0.32 | |
| MgO | 4.02% | 0.21 | |
| Na2O | 13.55% | 0.46 | |
| K2O | 0.10% | - | |
| Al2O3 | 0.50% | 0.01 | |
| SiO2 | 72.79% | 2.57 | |
| Fe2O3 | 0.10% | - | |
| SO3 | 0.30% | n/a | |
| Oxide Weight | 211.41 | ||
| Formula Weight | 212.05 | ||