Stain 6006

Description: Deep Crimson (CrSn)

Notes

Old number: 183

Related Information

Each Mason stain has its own personality for coloring the body


Multi-colored porcelain chips (blue, yellow, green, brown, black, pink)

This picture has its own page with more detail, click here to see it.

These Mason stains make the porcelain more refractory, but some more so (e.g. 6385, 6226). Some do not develop the intended color (e.g. 6006 pink, it is a glaze stain only). Some need a higher concentration (e.g. 6121, 6385). Some need a lower concentration (e.g. 6134). Some do not impart a homogeneous color (e.g. 6385). The data sheets from the stain manufacturer normally make it clear which of their stains are suitable in bodies. But it is up to you to test concentrations needed to get the desired color and what adjustments to the porcelain are needed to compensate its degree of vitrification in response to the effects of the stain.

Same glaze, same stain percentages

Yet two stains give completely different results


A bright red matte glaze

This picture has its own page with more detail, click here to see it.

Why does the red color not develop in the center glaze? This host recipe does not have the needed chemistry to develop the #6006 chrome-tin color (Mason Colors provide glaze unity formula guidelines: 6.7–8.4% CaO and avoiding MgO). This glaze recipe calculates to 9.8% CaO and 5% MgO. The MgO is the likely reason the red fails to develop. Yet this glaze produces excellent color with #6021 encapsulated stain (right). It isn't automatic that a strong red is achieved at just 5% encapsulated stain. The color is embedded in zircon crystals and aggressively melting KNaO, which this base recipe has very little of, attacks them and reduces color intensity.

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
Recipes GR6-L - Ravenscrag Cone 6 Transparent Burgundy
A stain-based method to achieve this color using the Ravenscrag base recipe.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy