Sodium Carbonate

Alternate Names: Soda Ash, Sodium Caronate Monohydrate, Na2CO3

Description: The most common form of sodium carbonate

Formula: Na2CO3 H2O or Na2O.CO2.H2O

Oxide Analysis Formula Tolerance
Na2O 50.00% 1.00
CO2 35.48%n/a
H2O 14.52%n/a
Oxide Weight 62.00
Formula Weight 124.00

Notes

The soda ash that the ceramic industry knows is a refined fine granular white material. It is very pure chemically and has been calcined (often referred to as dense soda ash). Grades (light, natural and dense) differ in the percentage of crystal water, particle sizes and bulk densities (the light grade has around 40 lbs/cubic foot, whereas dense is around 70). The dense grade may still lose up to 3% of it weight if calcined to about 400F.

The common ceramic use of soda ash is as a soluble deflocculant in ceramic slips and glazes. It works well in combination with sodium silicate to produce body slips that do not gel too quickly and whose rheology can be adjusted for changes in the hardness of the water (e.g. talc/ball clay body requires about 0.55% sodium silicate and 0.18% soda ash by weight of the clay powder, that would be 125g/40g). Higher soda ash proportions (vs sodium silicate) will produce a slip that gives a softer cast (stays wet longer). The total soda ash and sodium silicate amount should be tuned to create a slip that will eventually gel if left to stand. This thixotropic behavior will prevent it from settling. Sodium carbonate is also used for thinning glaze slurries.

Soda ash is not normally used as a source of Na2O in glazes because it is soluble. However, it is used as a key source of sodium in frits and glass. Its solubility makes it an ideal flux for Egyptian paste glazes. Although soda ash is a pure source of soda, a powerful flux in ceramics, by itself the powder of the dense version only begins caking at 1500F.

Soda ash production goes back to ancient times. Today, it is refined from Trona ore in the US (where the largest deposits are found). The ore is calcined, dissolved, and re-crystallized (other processes are used in other parts of the world). Soda ash is used in a very wide range of industries (glass is the single biggest user) so its chemical, physical and bulk properties are well understood and documented (General Chemical Industrial Products publishes an excellent booklet describing soda ash).

Monohydrate soda ash has 14.5% crystal water. This material is a textbook study of solubility and decomposition physics.
The individual crystals are fragile and handling equipment has to take this into account to preserve the grade.
It is not considered toxic, although micron-sized particles can be generated during handling.
Caking can occur during storage if the material absorbs water from the air. Baking soda is sodium bicarbonate, soda ash + carbon dioxide.

Related Information

50 lb bag of soda ash (or sodium carbonate).


This picture has its own page with more detail, click here to see it.

Soda Ash is soluble and is thus not useful in most ceramic glazes. However that very solubility makes it very useful to control the electrolytics of ceramic slurries. This is the dense variety, non-hydrous.

Back side of a bag of sodium carbonate (soda ash).


This picture has its own page with more detail, click here to see it.

Causes eye irritation. Prolonged contact with skin may cause irritation.

Links

URLs http://minerals.usgs.gov/minerals/pubs/commodity/soda_ash/
Statictics and Information
URLs http://images.dharmatrading.com/pdf/MSDS/soda-ash.pdf
Sample sodium carbonate data sheet
URLs http://www.sodaash.com
www.sodaash.com
URLs http://en.wikipedia.org/wiki/Sodium_carbonate
Sodium Carbonate at WikiPedia
Temperatures Sodium Carbonate decomposes (850-)
Temperatures Sodium Carbonate Dehydrates (370-)
Materials Sodium Bicarbonate
Materials Sodium Hydroxide
Materials Sodium Silicate
A sticky, viscous liquid. The most common deflocculant used in ceramics. Also used as a bonding agent.
Materials Sodium Carbonate Decahydrate
Materials Sodium Nitrate
Hazards Sodium Carbonate Toxicology
Typecodes Generic Material
Generic materials are those with no brand name. Normally they are theoretical, the chemistry portrays what a specimen would be if it had no contamination. Generic materials are helpful in educational situations where students need to study material theory (later they graduate to dealing with real world materials). They are also helpful where the chemistry of an actual material is not known. Often the accuracy of calculations is sufficient using generic materials.
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

Data

Frit Softening Point 851C M
Density (Specific Gravity) 1.44

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy