Alternate Names: Washing Soda, Hydrous Sodium Carbonate
Formula: Na2CO3.10H2O
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 21.68% | 1.00 | |
| CO2 | 15.38% | n/a | |
| H2O | 62.94% | n/a | |
| Oxide Weight | 62.00 | ||
| Formula Weight | 285.98 | ||
| Materials |
Sodium Carbonate
|
| Materials |
Sodium Carbonate Heptahydrate
|
| Materials |
Sodium Bicarbonate
|
| Typecodes |
Electrolyte
Materials used to control slurry properties of glazes and slips (vicosity, specific gravity). |
| Hazards |
Sodium Carbonate Toxicology
|
| Frit Softening Point | 34C D |
|---|---|
| Density (Specific Gravity) | 1.44 |