Pemco Frit P-991

Alternate Names: Frit 991, Frit P991

Description: All-fritted base for high talc bodies cone 02-2

Oxide Analysis Formula Tolerance
CaO 6.40% 0.27
K2O 3.70% 0.09
Na2O 9.00% 0.34
ZnO 10.30% 0.30
B2O3 5.00% 0.17
Al2O3 13.90% 0.32
SiO2 51.70% 2.02
Oxide Weight 235.26
Formula Weight 235.26

Related Information

Links

Materials Fusion Frit FZ-14
Materials Pemco Frit P-1J81
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials General Frit GF-104
Materials Hommel Frit 2GF27D
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.9x10-6 (50-450C)
Frit Melting Range (C) 1500-1670F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy