Odenwalder Clay

Alternate Names: Oldenwaelder, Odenwälder

Description: High iron low melting clay

Oxide Analysis Formula Tolerance
SiO2 58.40% 6.65
Al2O3 17.00% 1.14
TiO2 0.80% 0.07
Fe2O3 9.20% 0.39
CaO 1.00% 0.12
MgO 2.60% 0.44
K2O 5.70% 0.41
Na2O 0.20% 0.02
LOI 5.00%n/a
Oxide Weight 649.66
Formula Weight 683.85

Notes

Mined in the south-western part of Germany, it is said to be excellent for brown slips and glazes.
Sometimes compared to Albany Slip however it has a little less fluxing oxides, higher Al2O3 and a higher iron content (their datasheet claims 3.3% porosity at cone 04 whereas Albany is close to 20%, 8.5% fired shrinkage whereas Albany is around 2.5%).

The analysis provided by Carl-jaeger.de added up to 101 without the LOI, we have scaled it back to 95 to allow for the LOI.

Particle size:
< 63 µm 96 %
< 40 µm 91 %
< 20 µm 82 %
< 10 µm 71 %
< 6 µm 61 %
< 2 µm 39 %
< 1 µm 30 %
< 0.5 µm 22 %
D 50 Wert 0,00 µm

Related Information

Links

Materials Alberta Slip
Albany Slip successor - a plastic clay that melts to dark brown glossy at cone 10R, with a frit addition it can also host a wide range of glazes at cone 6.
Materials Albany Slip
A pure low plasticity clay that, by itself, melted to a glossy dark brown glaze at cone 10R. It was a popular glaze ingredient for many decades.
Materials Fremington Clay
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

Data

Frit Softening Point 1170C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy