Fremington Clay

Description: CLAY

Oxide Analysis Formula Tolerance
CaO 4.87% 0.37
K2O 3.98% 0.18
MgO 3.97% 0.42
Na2O 0.44% 0.03
TiO2 0.94% 0.05
Al2O3 20.11% 0.84
SiO2 59.68% 4.23
Fe2O3 6.01% 0.16
Oxide Weight 425.99
Formula Weight 425.99

Notes

High iron clay sold as a glaze ingredient.

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
Materials Albany Slip
A pure low plasticity clay that, by itself, melted to a glossy dark brown glaze at cone 10R. It was a popular glaze ingredient for many decades.
Materials Odenwalder Clay

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy