Kaolin A

Oxide Analysis Formula Tolerance
K2O 2.20% 0.07
TiO2 0.10% -
Fe2O3 0.80% 0.01
Al2O3 35.00% 1.00
SiO2 51.00% 2.47
LOI 11.30%n/a
Oxide Weight 259.66
Formula Weight 292.74

Related Information

Links

Materials Feldspar
In ceramics, feldspars are used in glazes and clay bodies. They vitrify stonewares and porcelains. They supply KNaO flux to glazes to help them melt.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.