Description: Dorset brown burning ball clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.30% | 0.02 | |
| K2O | 3.10% | 0.12 | |
| MgO | 0.40% | 0.03 | |
| Na2O | 0.50% | 0.03 | |
| TiO2 | 1.20% | 0.05 | |
| Al2O3 | 29.00% | 1.00 | |
| SiO2 | 54.00% | 3.16 | |
| Fe2O3 | 2.30% | 0.05 | |
| LOI | 8.50% | n/a | |
| Oxide Weight | 319.37 | ||
| Formula Weight | 349.03 | ||
A highly plastic clay that vitrifies at very low temperatures (much lower than its chemistry suggests). It has an exceptionally small particle size. Fires brown, having almost 2% Fe2O3.
| Materials |
Ball Clay
A fine particled highly plastic secondary clay used mainly to impart plasticity to clay and porcelain bodies and to suspend glaze, slips and engobe slurries. |
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |