Hommel Frit 482

Description: Barium zinc frit

Oxide Analysis Formula Tolerance
K2O 3.24% 0.09
Na2O 5.31% 0.23
CaO 2.27% 0.11
MgO 3.41% 0.23
BaO 4.13% 0.07
ZnO 6.96% 0.23
PbO 3.36% 0.04
Al2O3 12.60% 0.33
B2O3 3.19% 0.12
SiO2 54.82% 2.45
TiO2 0.71% 0.02
Oxide Weight 268.37
Formula Weight 268.37

Related Information

Links

Materials Pemco Frit Pb-1279
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.0 x 10-6
Frit Softening Point 1750F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy