Description: CALCIUM ZIRCONIUM SILICATE
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 23.43% | 1.00 | |
| ZrO2 | 51.46% | 1.00 | |
| SiO2 | 25.10% | 1.00 | |
| Oxide Weight | 239.41 | ||
| Formula Weight | 239.41 | ||
Was used in high fire glazes as the sole opacifier. It can be blended with other zirconium products for special finishes.
It is no longer manufactured.
This was an ideal opacifier for use in chrome-tin pink and maroon glazes since the calcium enhanced the development of the color.
| Typecodes |
Opacifier
Opacifiers are powders that turn transparent glazes opaque by various chemical and physical mechanisms (and combinations of mechanisms). |
| Materials |
Zircon
Zircon (zirconium silicate) is a hard, dense, refractory ceramic material used to opacify pottery glazes and in refractory products such as kiln washes, crucibl |