Oxide Analysis Formula Tolerance
SiO2 61.50% 4.16
Al2O3 25.10% 1.00
Fe2O3 1.00% 0.03
CaO 0.06% -
MgO 0.77% 0.08
TiO2 1.27% 0.06
Na2O 0.16% 0.01
K2O 2.88% 0.12
LOI 7.29%n/a
Oxide Weight 376.87
Formula Weight 406.51

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.
Materials Ball Clay
A fine particled highly plastic secondary clay used mainly to impart plasticity to clay and porcelain bodies and to suspend glaze, slips and engobe slurries.
URLs http://www.walkerceramics.com.au/Raw Mat'l typical_analysis.htm
Walker Ceramics materials

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy