1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Australian Spodumene

Alternate Names: Ausi Spodumene, Ausi Spod

Formula: Li2O.Al2O3.4SiO2

Oxide Analysis Formula Tolerance
Li2O 7.60% 0.98 0.25
K2O 0.08% - 0.25
Na2O 0.15% 0.01 max
P2O5 0.17% - 0.40
CaO 0.05% - 0.90
SiO2 64.50% 4.12
Fe2O3 0.07% - max
MnO 0.02% - max
Al2O3 26.50% 1.00
TiO2 0.01% -
LOI 0.20%n/a
Oxide Weight 380.77
Formula Weight 381.54

Notes

Australian spodumenes are considered the whitest in the world.

The materials feature [Si2O6]3- chains bonded together by lithium and aluminum ions. It is a monoclinic pyroxene in the form of long tabular, prismatic crystals.

Beta-spodumene (formed at 1082C) has a very low coefficient of thermal expansion, about 1 x 10-6/°C for the range 25°C to 1000°C.

Related Information

Here is why Spodumene powder glistens in the light


Why Spodumene powder glistens in the light

This picture has its own page with more detail, click here to see it.

Spodumene ceramic grade, used in glazes, is a 200 mesh material. How could the particles be big enough to glisten in the light? This is a micrograph of some of the particles from the 0.6% plus 100 mesh material that I extracted in a particle size distribution test. And 8% is plus 200 mesh. And all that material is flakey like this, millions of tiny mirrors. This also explains why the material becomes airborne so easily and why it is really really not good to breathe this stuff in.

Links

URLs http://www.amalgamet.com/Products/minerals.htm
Description of material
Materials SC7.0 Spodumene
Materials Foote Spodumene
Materials Spodumene
Spodumene is a lithium sourcing feldspar, an alternative to lithium carbonate to supply Li2O to ceramic glazes. Contains up to about 8% Li2O.
Materials Spodumene Concentrate
Materials CGS 3.1 Spodumene
Materials SC 1.1 Spodumene
Materials SC 1.2 Spodumene
Materials UGS Spodumene
Materials FSC 2.1 Spodumene
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

Data

Hardness (Moh) 6-5-7
Frit Softening Point 1420C
Density (Specific Gravity) 3.2

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy