General Frit GF-114

Alternate Names: Frit 114, Frit GF114

Description: Leadless High Expansion

Oxide Analysis Formula Tolerance
CaO 0.50% 0.03
K2O 5.40% 0.18
Na2O 14.70% 0.76
ZnO 0.70% 0.03
B2O3 16.90% 0.78
Al2O3 12.10% 0.38
SiO2 49.70% 2.65
F 1.80% 0.30
Oxide Weight 326.35
Formula Weight 326.35

Notes

High expansion for crackle low temperature all-fritted and partially-fritted tile glazes.

Related Information

Links

Materials Hommel Frit 25
Materials Fusion Frit F-225
Materials Ferro Frit 3269
Materials Fusion Frit FZ-25
Materials Pemco Frit P-25
Materials Hommel Frit 259
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 10.00
Frit Softening Point 1370F