Fusion Frit FZ-30

Alternate Names: Fusion Frit FZ30

Description: Zinc barium artware, tile, sanitaryware glaze frit

Oxide Analysis Formula Tolerance
K2O 4.00% 0.11
Na2O 1.40% 0.06
BaO 8.50% 0.14
SrO 7.50% 0.19
ZnO 16.00% 0.50
Al2O3 1.00% 0.03
B2O3 11.50% 0.42
SiO2 39.60% 1.69
ZrO2 10.50% 0.22
Oxide Weight 256.78
Formula Weight 256.78

Related Information

Links

Materials Ferro Frit 3240
Materials Hommel Frit G-26
Materials Pemco Frit P-64
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 69
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.47 x 10-6
Frit Softening Point 1550F