Oxide Analysis Formula Tolerance
BaO 7.90% 0.11
CaO 8.80% 0.33
K2O 0.60% 0.01
Na2O 4.50% 0.15
ZnO 15.80% 0.40
ZrO2 10.20% 0.17
B2O3 10.00% 0.30
Al2O3 0.90% 0.02
SiO2 39.50% 1.37
F 1.90% 0.21
Oxide Weight 207.91
Formula Weight 207.91

Related Information

Links

Materials Pemco Frit P-64
Materials Fusion Frit FZ-30
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit G-26
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.60
Frit Melting Range (C) 1500F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy