March 2026: We are doing major upgrades to code here, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.
| Monthly Tech-Tip | Feb 14-15, 2026 - Major Server Upgrade Done | No tracking! No ads! |
Alternate Names: Frit FZ22
Description: Zinc barium calcium frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 4.10% | 0.05 | |
| CaO | 14.30% | 0.48 | |
| K2O | 4.00% | 0.08 | |
| MgO | 0.60% | 0.03 | |
| Na2O | 1.60% | 0.05 | |
| ZnO | 13.20% | 0.31 | |
| B2O3 | 4.50% | 0.12 | |
| Al2O3 | 8.20% | 0.15 | |
| SiO2 | 49.30% | 1.56 | |
| Oxide Weight | 189.39 | ||
| Formula Weight | 189.39 | ||
| Materials |
Pemco Frit P-586
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 1030
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |