Hommel Frit 400

Description: Leadless barium frit

Oxide Analysis Formula Tolerance
BaO 27.70% 0.67
Na2O 5.50% 0.33
B2O3 12.34% 0.66
Al2O3 5.40% 0.20
SiO2 49.05% 3.03
Oxide Weight 371.16
Formula Weight 371.16

Related Information

Links

Materials General Frit GF-129
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3289
Materials Pemco Frit P-626
Materials Fusion Frit F-65
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.90
Co-efficient of Linear Expansion 7.9 x 10-6
Frit Softening Point 1570F
Frit Melting Range (C) 1570F