Ferro Frit 3560

Description: Very low lead zinc barium frit

Oxide Analysis Formula Tolerance
BaO 3.95% 0.06
CaO 6.99% 0.29
MgO 2.08% 0.12
K2O 3.64% 0.09
Na2O 5.06% 0.19
ZnO 7.69% 0.22
PbO 2.88% 0.03
Al2O3 12.70% 0.29
B2O3 2.09% 0.07
SiO2 52.92% 2.05
Oxide Weight 232.77
Formula Weight 232.77

Related Information

Links

Materials Fusion Frit FZ-6
Materials Pemco Frit Pb-1279
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.6
Frit Melting Range (C) 1700F