Container Glass

Oxide Analysis Formula Tolerance
SiO2 74.30% 3.03
Al2O3 1.30% 0.03
MgO 0.20% 0.01
CaO 10.50% 0.46
Na2O 13.20% 0.52
K2O 0.30% 0.01
Oxide Weight 244.48
Formula Weight 244.48