Alternate Names: Frit CC-274-2
Description: Low alumina strontium boron frit
Oxide | Analysis | Formula | Tolerance |
---|---|---|---|
SiO2 | 57.50% | 3.51 | 2.5 |
B2O3 | 12.50% | 0.66 | 2.5 |
Na2O | 2.50% | 0.15 | 2.5 |
K2O | 2.50% | 0.10 | 2.5 |
CaO | 7.50% | 0.49 | 2.5 |
SrO | 7.50% | 0.27 | 2.5 |
Al2O3 | 7.50% | 0.27 | 2.5 |
Oxide Weight | 357.21 | ||
Formula Weight | 357.21 |
This is a USA pottery frit, Ferro now calls it Frit CC-274-2. This is very similar to Fusion frit 524 except that it does not have the 2% BaO.
As of 2008 Ferro only provides an approximate analysis, but the one here is historical (from previous sources).
Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
Materials |
Fusion Frit F-524
A low fire base glaze, add 10% kaolin, adjust thermal expansion using other frits. |
Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
Typecodes |
Available from Laguna Clays
|
URLs |
https://digitalfire.com/4sight/datasheets/ferropotteryfrits2008.pdf
Ferro Pottery Frits 2008 |
Co-efficient of Linear Expansion | 7.19 |
---|---|
Frit Melting Range (C) | 1850F |