Degussa Frit 90208

Description: Very high sodium, boron free, high expansion frit

Oxide Analysis Formula Tolerance
Na2O 28.89% 1.00
Al2O3 9.51% 0.20
SiO2 61.61% 2.20
Oxide Weight 214.63
Formula Weight 214.63

Notes

Commonly used to make crystalline glazes because of the high sodium and relatively low alumina (Al2O3) contents. However other similar frits have much lower Al2O3.

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Fusion Frit F644
Materials Mondre and Manz Frit 1233
Materials Glasurfritten M1233
Materials Moulin Fritte M1233
Materials Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts a very low temperatures.

Data

Co-efficient of Linear Expansion 123 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 458C
Heating Microscope Analysis for Frits 685C
Heating Microscope Analysis for Frits 890C