1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Glasurfritten M1233

Alternate Names: M 1233,M-1233

Description: Very high alkali, zero boron, low alumina, high expansion frit

Oxide Analysis Formula Tolerance
CaO 7.80% 0.30
K2O 13.00% 0.30
Na2O 11.40% 0.40
Al2O3 1.40% 0.03
SiO2 66.40% 2.40
Oxide Weight 216.96
Formula Weight 216.96

Notes

Commonly used to make crystalline glazes because of the very high alkali and very low alumina contents.

Related Information

Links

Materials Mondre and Manz Frit 1233
Materials Moulin Fritte M1233
Materials Degussa Frit 90208
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 141 x 10-7
Frit Softening Point 503C
Frit Melting Range (C) 800-1080C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy