Mondre and Manz Frit 1233

Alternate Names: Alkalifritte C-1233, Alkalifritte M 1233, Fritte M1233

Description: Very high alkali, zero boron, low alumina, high expansion frit

Oxide Analysis Formula Tolerance
CaO 7.75% 0.30
Na2O 11.42% 0.40
SiO2 66.41% 2.40
K2O 13.01% 0.30
Al2O3 1.41% 0.03
Oxide Weight 217.18
Formula Weight 217.18

Notes

Commonly used to make crystalline glazes because of the very high alkali and very low alumina contents.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Glasurfritten M1233
Materials Moulin Fritte M1233
Materials Degussa Frit 90208
Materials Fusion Frit F644
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 503C