1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Granular Ilmenite

Alternate Names: Illmenite Granular, Granular Illmenite, Granular Iron Titanate

Related Information

Original Container bag of Granular Ilmenite


This picture has its own page with more detail, click here to see it.

Illmenite Granular in a porcelain clay body


This picture has its own page with more detail, click here to see it.

Fired at cone 6. This grade of illmenite is about 17% between 70 and 100 mesh, the rest in finer than 100 mesh. By Garret Schipper.

0.02% manganese, ilmenite, rutile granular in a buff stoneware at cone 6


This picture has its own page with more detail, click here to see it.

Clearly, the manganese is blossoming and producing far better speckle than the other two.

Links

Oxide Analysis Formula Tolerance
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
Materials Granular Rutile
The same material as milled rutile, but ground only to granular size.
Materials Ilmenite
Materials Manganese Granular
In ceramics, it is used primarily in clays and glazes to achieve fired speckle (including the brick industry).
Materials Magnetite Granular

Mechanisms

Glaze VariegationIllmenite granular is available in a variety of particle sizes and can be employed to add speckle to glazes. Start with about 0.2%.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy