CGS 3.1 Spodumene

Description: Glass Grade Spodumene

Oxide Analysis Formula Tolerance
Li2O 5.00% 0.96
Fe2O3 0.10% -
Al2O3 18.50% 1.03
SiO2 75.00% 7.11
Na2O 0.25% 0.02
K2O 0.35% 0.02
LOI 0.30%n/a
Oxide Weight 565.14
Formula Weight 566.84

Related Information

Links

URLs http://www.amalgamet.com/Products/minerals.htm
Description of material
Materials Spodumene Concentrate
Materials Foote Spodumene
Materials Spodumene
Spodumene is a lithium sourcing feldspar, an alternative to lithium carbonate to supply Li2O to ceramic glazes. Contains up to about 8% Li2O.
Materials Australian Spodumene
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

Data

Hardness (Moh) 6-5-7
Frit Softening Point 1420C
Sieve Analysis Dry Tyler 150 mesh: 95%
Density (Specific Gravity) 3.2