Hectabrite

Alternate Names: Hectabrite DP

Description: Hydroclassified Hectorite

Oxide Analysis Formula Tolerance
SiO2 61.80% 1.33
Al2O3 1.58% 0.02
MgO 20.30% 0.65
Fe2O3 1.23% 0.01
CaO 10.10% 0.23
Na2O 2.80% 0.06
Li2O 1.29% 0.06
K2O 0.33% -
LOI 4.50%n/a
Oxide Weight 128.18
Formula Weight 134.22

Notes

White magnesium-rich surface-modified sodium hectorite clay highly purified to exhibit rheology four to five times more efficient than ground bentonite.

Hectabrite AW is a flake material which exhibits excellent emulsification, thickening and suspension properties at low solids levels. It is mostly used in pharmaceuticals, cosmetics and personal care products.

Hectabrite DP is a free-flowing powder. Used as a binder and plasticizer in ceramic bodies. In glazes gels and reduces settling.

Related Information

Links

Materials Hectorite
A sodium magnesium montmorillonite that burns much whiter than bentonite (because of lower iron content).
Materials Polargel
Materials Volclay Bentonite
Materials Hectalite 200
Materials Magnabrite
Materials Veegum
A clay of incredibly small particle size. It has the highest plasticity of any known clay and acts as a suspending and gelling agent in slurries.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy