Polargel

Description: Purified Bentonites

Notes

Naturally occurring white sodium bentonite with fine texture and brilliant white color

Polargel® IVP (Patented Intercalated Clay Technology)
Mixes well with water to provide gel stability and integrity in polar solvents, silicon oils and acidic or alkaline compounds for simplifying
formulations-the next generation of thixotropes!

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Hectalite 200
Materials Hectabrite
White magnesium-rich surface-modified highly purified sodium hectorite clay 4-5 times more efficient than raw bentonite.
Materials Bentonite
Bentonite can make a clay body instantly plastic, only 2-3% can have a big effect. It also suspends slurries so they don't settle out and slows down drying.
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy